How Wood Hardness is Measured

Science Woodworking
How Wood Hardness is Measured

In fact, there are now a couple of different procedures, but the traditional method is known as the “Janka hardness test,” named for Austrian wood researcher Gabriel Janka, who invented it in 1906. The test measures the force required to embed a standard-sized steel ball (0.444in/11.28mm diameter) exactly halfway into the surface of a standard-sized sample of the wood. The formal procedure, embodied since 1927 as ASTM standard D143, is not freely available, but J.J. Morlan summarizes the key points well:

Testing is done on wood from the trunk of the tree and is almost always the heartwood. With heartwood there are a handful of exceptions. One that comes to mind is Balsa {Ochroma pyramidale}. Balsa is always milled from sapwood. The standard sample as indicated in ASTM D 143 is to be at 12% moisture content, be clear {no knots}, a solid block of wood having the dimensions of at least 2″ x 2″ x 6″ long and the rate of loading will be machine set at 1/4″ per minute. Two indentations are made on the tangential surface and two indentations on the radial surface. The four indentations are then added together and divided by 4 to get the average value of the force, with the result being declared as the side hardness.When testing is done on a piece of wood with the force applied to the end grain surface, the test is of end hardness. The end hardness of wood/lumber/timber will almost always be higher {harder} than its side hardness.

Morlan also provides a lengthy list of Janka hardness values for various woods, of which the current record holder is Allocasuarina luehmannii, aka “Australian bull-oak,” which require 2.5 tons of pressure. By comparison, Ponderosa pine tests at 480 lbs on the Janka scale, and low-density balsa wood at 88 lbs. The world’s softest wood, by Janka hardness, is Cavanillesia platanifolia, aka “quipo,” at 22 lbs. The Forestry Service research note linked below gives a good historical background and general overview of the Janka test.

Janka Hardness Using Nonstandard Specimens (PDF)

4 thoughts on “How Wood Hardness is Measured

  1. Wood "hardness" simple tests (pic heavy...!) - Page 2 - International Association of Penturners says:

    […] find it today. Not this Australian man’s testing method should meet with your approval. How Wood Hardness is Measured | MAKE For those that find this thread getting weary but want to know how hard your wood is check out […]

  2. Janka – an important measurement of wood you probably never heard of says:

    […] Test photos courtesy of: https://makezine.com/ and […]

  3. Janka – an important measurement of wood you probably never heard of – RoRoCo.Co says:

    […] Test photos courtesy of: https://makezine.com/ and […]

  4. Tips for Choosing the Best Wood Floor Color for Your Home says:

    […] wood floor color, you need to select the proper material. That includes its hardness. The Janka Hardness Scale rates wood’s hardness. As we explained in the blog, a wood’s hardness is determined by […]

Comments are closed.

Discuss this article with the rest of the community on our Discord server!
Tagged

I am descended from 5,000 generations of tool-using primates. Also, I went to college and stuff. I am a long-time contributor to MAKE magazine and makezine.com. My work has also appeared in ReadyMade, c't – Magazin für Computertechnik, and The Wall Street Journal.

View more articles by Sean Michael Ragan

ADVERTISEMENT

Maker Faire Bay Area 2023 - Mare Island, CA

Escape to an island of imagination + innovation as Maker Faire Bay Area returns for its 15th iteration!

Buy Tickets today! SAVE 15% and lock-in your preferred date(s).

FEEDBACK